Temperature Range, K: 300-3540
Composition (weight percent), Specifications and Remarks: Tungsten filaments aged 24 hrs at 2400 K; measured in vacuum; smoothed values.
Source for Curve 1
Data originally published at 10.1103/PhysRev.7.302. Tabulated data extracted from Y. S. Touloukian and D. P. DeWitt, *Thermal Radiative Properties: Metallic Elements and Alloys*, Thermophysical Properties of Matter - The TPRC Data Series, Volume 7, IFI/Plenum, New York, 1970; table 231, curve 27. Digital version served at EKHI (https://thermomat.ehu.eus/ekhi).